Oil paste is essential for any post-firing repairs. It can also be used to combine previously fired pieces. Requires piece(s) to be re-fired at 1472 F, although a butane torch may be used when joining fine silver bezel wire seams.
Also includes handy thinner to make oil paste easily workable. 10 gm of each. Weights are post-fire. Shrinks 8 - 10% during firing.
Pendant below by Jackie Truty. From "Art Clay Silver and Gold" book #6979
|